Effect of Bi4Ti3O12 on microstructure and piezoelectric properties of 0.1BiYbO3-0.9PbTiO3 ceramics

Feng Gao, Hong Li Liu, Bo Zhang, Le Yang, Chang Sheng Tian

科研成果: 期刊稿件文章同行评审

摘要

In this paper, piezoelectric ceramics 0.1BiYbO3-0.9PbTiO3 (BYPT) with high Curie temperature were prepared by using Bi4Ti3O12 (BIT) as raw material. The effect of BIT content on the microstructure and electrical properties of BYPT ceramics was investigated. The results showed that the optimized sintering temperature was 1140°C. There were many phases coexisting in the BYPT ceramics with Curie temperature higher than 520°C. The Curie temperature TC, the piezoelectric coefficient d33 and the dielectric constant ε increased firstly and then decreased with increasing BIT content. The BYPT2 ceramic had the highest Curie temperature and piezoelectric constant.

源语言英语
页(从-至)86-89
页数4
期刊Yadian Yu Shengguang/Piezoelectrics and Acoustooptics
32
1
出版状态已出版 - 2月 2010

指纹

探究 'Effect of Bi4Ti3O12 on microstructure and piezoelectric properties of 0.1BiYbO3-0.9PbTiO3 ceramics' 的科研主题。它们共同构成独一无二的指纹。

引用此