In this paper, piezoelectric ceramics 0.1BiYbO3-0.9PbTiO3 (BYPT) with high Curie temperature were prepared by using Bi4Ti3O12 (BIT) as raw material. The effect of BIT content on the microstructure and electrical properties of BYPT ceramics was investigated. The results showed that the optimized sintering temperature was 1140°C. There were many phases coexisting in the BYPT ceramics with Curie temperature higher than 520°C. The Curie temperature TC, the piezoelectric coefficient d33 and the dielectric constant ε increased firstly and then decreased with increasing BIT content. The BYPT2 ceramic had the highest Curie temperature and piezoelectric constant.

Original languageEnglish
Pages (from-to)86-89
Number of pages4
JournalYadian Yu Shengguang/Piezoelectrics and Acoustooptics
Volume32
Issue number1
StatePublished - Feb 2010

Keywords

  • Curie temperature
  • Dielectric properties
  • Microstructure
  • Piezoelectric ceramics

Fingerprint

Dive into the research topics of 'Effect of Bi4Ti3O12 on microstructure and piezoelectric properties of 0.1BiYbO3-0.9PbTiO3 ceramics'. Together they form a unique fingerprint.

Cite this