Atomic Layer Deposition of a Pt-Skin Catalyst for Base-Free Aerobic Oxidation of 5-Hydroxymethylfurfural to 2,5-Furandicarboxylic Acid

Jinshan Shen, Hao Chen, Kequan Chen, Yong Qin, Xiuyang Lu, Pingkai Ouyang, Jie Fu

科研成果: 期刊稿件文章同行评审

45 引用 (Scopus)

摘要

A Pt-Ni/AC bimetallic catalyst was prepared by atomic layer deposition of Pt nanoparticles on the surface of Ni/AC for base-free oxidation of 5-hydroxymethylfurfural (5-HMF) to 2,5-furandicarboxylic acid (2,5-FDCA). A comparison of the Pt-Ni bimetallic catalyst with Ni and the Pt monometallic catalyst was demonstrated by X-ray diffraction (XRD), transmission electron microscopy (TEM), and temperature-programmed desorption of CO (CO-TPD). Compared with the Ni/AC and Pt/AC (1.6 wt % Pt) catalysts, the bimetallic Pt-Ni/AC catalyst had a higher activity for the oxidation of 5-HMF to 2,5-FDCA, with only a 0.4 wt % Pt loading. A 97.5% yield of 2,5-FDCA with 100% 5-HMF conversion was obtained after 15 h at 100 °C. A mass-based activity value of 35.8 h-1 was obtained over the Pt-Ni/AC-15ALD catalyst. The combination of Pt with Ni increased the ability of Pt for C - O adsorption and oxidation, thus increasing the activity of the Pt catalyst. Finally, the catalyst showed good reusability for at least four times without any reduction in the catalytic activity.

源语言英语
页(从-至)2811-2818
页数8
期刊Industrial and Engineering Chemistry Research
57
8
DOI
出版状态已出版 - 28 2月 2018
已对外发布

指纹

探究 'Atomic Layer Deposition of a Pt-Skin Catalyst for Base-Free Aerobic Oxidation of 5-Hydroxymethylfurfural to 2,5-Furandicarboxylic Acid' 的科研主题。它们共同构成独一无二的指纹。

引用此