Atomic Layer Deposition of a Pt-Skin Catalyst for Base-Free Aerobic Oxidation of 5-Hydroxymethylfurfural to 2,5-Furandicarboxylic Acid

Jinshan Shen, Hao Chen, Kequan Chen, Yong Qin, Xiuyang Lu, Pingkai Ouyang, Jie Fu

Research output: Contribution to journalArticlepeer-review

45 Scopus citations

Abstract

A Pt-Ni/AC bimetallic catalyst was prepared by atomic layer deposition of Pt nanoparticles on the surface of Ni/AC for base-free oxidation of 5-hydroxymethylfurfural (5-HMF) to 2,5-furandicarboxylic acid (2,5-FDCA). A comparison of the Pt-Ni bimetallic catalyst with Ni and the Pt monometallic catalyst was demonstrated by X-ray diffraction (XRD), transmission electron microscopy (TEM), and temperature-programmed desorption of CO (CO-TPD). Compared with the Ni/AC and Pt/AC (1.6 wt % Pt) catalysts, the bimetallic Pt-Ni/AC catalyst had a higher activity for the oxidation of 5-HMF to 2,5-FDCA, with only a 0.4 wt % Pt loading. A 97.5% yield of 2,5-FDCA with 100% 5-HMF conversion was obtained after 15 h at 100 °C. A mass-based activity value of 35.8 h-1 was obtained over the Pt-Ni/AC-15ALD catalyst. The combination of Pt with Ni increased the ability of Pt for C - O adsorption and oxidation, thus increasing the activity of the Pt catalyst. Finally, the catalyst showed good reusability for at least four times without any reduction in the catalytic activity.

Original languageEnglish
Pages (from-to)2811-2818
Number of pages8
JournalIndustrial and Engineering Chemistry Research
Volume57
Issue number8
DOIs
StatePublished - 28 Feb 2018
Externally publishedYes

Fingerprint

Dive into the research topics of 'Atomic Layer Deposition of a Pt-Skin Catalyst for Base-Free Aerobic Oxidation of 5-Hydroxymethylfurfural to 2,5-Furandicarboxylic Acid'. Together they form a unique fingerprint.

Cite this