Thermal cycling damage mechanisms of C/SiC composites in displacement constraint and oxidizing atmosphere

科研成果: 期刊稿件文章同行评审

21 引用 (Scopus)

摘要

A constraint stress of 62.5 MPa is created on a three-dimensional C/SiC composite specimen whose both ends are fixed when temperature is cycled between 900° and 1200°C. The cyclic stress results in a maximum damage strain of 0.06% within 50 cycles owing to coating and matrix cracking, fiber debonding, sliding, and breaking in the composite. This constrained specimen elongation also leads to a final compressive stress of 14 MPa on the composite through a decrease in the baseline constraint stress. Wet oxygen atmosphere at a high cyclic temperature, concomitant with stresses, can aggravate the damage situation by alternate oxidation between internal and external fibers in composites.

源语言英语
页(从-至)2330-2334
页数5
期刊Journal of the American Ceramic Society
89
7
DOI
出版状态已出版 - 7月 2006

指纹

探究 'Thermal cycling damage mechanisms of C/SiC composites in displacement constraint and oxidizing atmosphere' 的科研主题。它们共同构成独一无二的指纹。

引用此