Structure and Oxidation Behavior of Zr–Y Modified Silicide Coatings Prepared on an Nb–Ti–Si–Cr Based Ultrahigh Temperature Alloy

Xuan Li, Xiping Guo, Yanqiang Qiao

科研成果: 期刊稿件文章同行评审

24 引用 (Scopus)

摘要

Zr–Y modified silicide coatings have been prepared on an Nb–Ti–Si–Cr based ultrahigh temperature alloy by a pack cementation process. The effects of amount of Zr powder in the pack mixture and co-deposition temperature on the coating structure were assessed. The coatings prepared at 1,250 °C with different amounts of Zr powders in the pack mixture have similar structures, mainly consisting of a thick (Nb,X)Si2 (X represents Ti, Cr and Hf elements) outer layer, a thin (Ti,Nb)5Si4 middle layer and a 1–2 µm thick (Nb,X)5Si3 inner layer. The increased amount of Zr powders in the pack mixtures led to a significant decrease in the coating thickness. The coatings prepared at 1,150 and 1,200 °C have similar structures to that prepared at 1,250 °C. However, when the co-deposition temperature increases to 1,300 and 1,350 °C, a (Ti,Nb)5Si3 outermost layer formed in addition to the three layers mentioned above. The Zr–Y modified silicide coating can protect the base alloy from oxidation at least for 100 h at 1,250 °C in air. The good oxidation resistance of the Zr–Y modified silicide coating is attributed to the formation of a dense scale consisting of SiO2 and TiO2.

源语言英语
页(从-至)253-271
页数19
期刊Oxidation of Metals
83
3-4
DOI
出版状态已出版 - 4月 2015

指纹

探究 'Structure and Oxidation Behavior of Zr–Y Modified Silicide Coatings Prepared on an Nb–Ti–Si–Cr Based Ultrahigh Temperature Alloy' 的科研主题。它们共同构成独一无二的指纹。

引用此