Stress corrosion cracking analysis under thermal residual stress field using S-FEM
Masanori Kikuchi, Yoshitaka Wada, Yuto Shmizu,
Yulong Li
民航学院
Tokyo University of Science
Suwa University of Science
科研成果
:
书/报告/会议事项章节
›
会议稿件
›
同行评审
5
引用 (Scopus)
综述
指纹
指纹
探究 'Stress corrosion cracking analysis under thermal residual stress field using S-FEM' 的科研主题。它们共同构成独一无二的指纹。
分类
加权
按字母排序
Engineering
Analytical Result
25%
Crack Closure
25%
Crack Growth
50%
Crack Growth Behavior
25%
Dimensional Analysis
25%
Experimental Result
25%
Fracture Behavior
25%
Growth Analysis
25%
Heat Affected Zone
50%
Integral Method
25%
Japan
25%
Nuclear Energy
25%
Residual Stress
75%
Stress Corrosion Cracking
100%
Stress Field
100%
Stress-Intensity Factor
25%
Thermal Residual Stress
100%
Thermal Stress
50%
Two Dimensional
25%
Material Science
Crack Closure
25%
Crack Growth
75%
Fracture Behavior
25%
Residual Stress
100%
Stress Corrosion Cracking
100%
Stress Field
100%
Stress Intensity Factor
25%
Thermal Stress
50%