TY - JOUR
T1 - Solidification microstructure of hypereutectic high chromium cast iron semi-solid slurry in centrifugal casting
AU - Huang, Zhifu
AU - Xing, Jiandong
AU - Zhang, Anfeng
AU - Huang, Weidong
PY - 2006/8
Y1 - 2006/8
N2 - The microstructure of annular parts in centrifugal casting has been observed, in which hypereutectic high chromium cast iron semi-solid slurry prepared by slope cooling body method is used. The results indicate that not only segregation phenomenon of primary carbide in the semi-solid structure but also sharp dividing line of the segregation, where the dividing line locates at the distance of about 6 mm from the radial outer face of the annular parts, can be observed. At the given experimental condition, the shrinkage porosity tendency in the structure can only be partially eliminated by centrifugal forces. The dividing line of shrinkage porosity appearance in the microstructure also locates at the distance of about 6mm from the radial outer of the annular one, that is, as the distance from the radial outer of the annular one is less than 6mm, there are no shrinkage porosities in the radial area, contrarily, there are shrinkage porosities.
AB - The microstructure of annular parts in centrifugal casting has been observed, in which hypereutectic high chromium cast iron semi-solid slurry prepared by slope cooling body method is used. The results indicate that not only segregation phenomenon of primary carbide in the semi-solid structure but also sharp dividing line of the segregation, where the dividing line locates at the distance of about 6 mm from the radial outer face of the annular parts, can be observed. At the given experimental condition, the shrinkage porosity tendency in the structure can only be partially eliminated by centrifugal forces. The dividing line of shrinkage porosity appearance in the microstructure also locates at the distance of about 6mm from the radial outer of the annular one, that is, as the distance from the radial outer of the annular one is less than 6mm, there are no shrinkage porosities in the radial area, contrarily, there are shrinkage porosities.
KW - Centrifugal casting
KW - Hypereutectic gigh chromium cast iron
KW - Microstructure segregation
KW - Semi-solid slurry
KW - Shrinkage porosity
UR - http://www.scopus.com/inward/record.url?scp=33749472205&partnerID=8YFLogxK
M3 - 文章
AN - SCOPUS:33749472205
SN - 1001-2249
VL - 26
SP - 489
EP - 491
JO - Tezhong Zhuzao Ji Youse Hejin/Special Casting and Nonferrous Alloys
JF - Tezhong Zhuzao Ji Youse Hejin/Special Casting and Nonferrous Alloys
IS - 8
ER -