Sluggish dendrite growth in substantially undercooled liquid Fe-Sb alloy

W. L. Wang, C. L. Shen, B. C. Luo, B. Wei

科研成果: 期刊稿件文章同行评审

3 引用 (Scopus)

摘要

Dendrite growth within substantially undercooled liquid alloys is usually characterised by a very high growth velocity, even over 100 m/s. Here we report that dendrite growth becomes quite sluggish in a highly undercooled liquid Fe-8.5wt.%Sb alloy because it has a broad solidification temperature range of 412 K. The measured growth velocity of the dendritic -Fe phase increases up to a maximum of only 1.38 m/s at 301 K undercooling. If this liquid alloy is undercooled further by 390 K (0.22TL), the dendrite growth velocity decreases gradually. A structural morphology transition from a coarse dendrite to an equiaxed grain takes place once undercooling exceeds 73 K. Energy dispersive spectroscopy analyses of the solute distribution reveal that solute trapping depends mainly on the actual dendrite growth velocity rather than the degree of undercooling.

源语言英语
页(从-至)409-418
页数10
期刊Philosophical Magazine Letters
89
7
DOI
出版状态已出版 - 7月 2009

指纹

探究 'Sluggish dendrite growth in substantially undercooled liquid Fe-Sb alloy' 的科研主题。它们共同构成独一无二的指纹。

引用此