Size effect of nickel-based single crystal superalloy revealed by nanoindentation with low strain rates
Xu Long
, Ziyi Shen, Jiao Li, Ruipeng Dong, Ming Liu,
Yutai Su
, Chuantong Chen
力学与土木建筑学院
Northwestern Polytechnical University Xian
Fuzhou University
The University of Osaka
科研成果
:
期刊稿件
›
文章
›
同行评审
47
引用 (Scopus)
综述
指纹
指纹
探究 'Size effect of nickel-based single crystal superalloy revealed by nanoindentation with low strain rates' 的科研主题。它们共同构成独一无二的指纹。
分类
加权
按字母排序
Engineering
Indentation
100%
Lower Strain Rate
100%
Single Crystal Superalloys
100%
Size Effect
100%
Strain Rate
50%
Strain Rate Effect
33%
Finite Element Simulation
33%
Loading Rate
33%
Finite Element Analysis
16%
Contact Area
16%
Good Agreement
16%
Dimensionless
16%
Characteristic Length
16%
Material Parameter
16%
Material Science
Strain Rate
100%
Superalloys
100%
Single Crystal
100%
Indentation
100%
Nanoindentation
100%
Finite Element Method
50%
Strain Rate Effect
33%
Contact Area
16%
Analytical Method
16%