SiC coating toughened by SiC nanowires to protect C/C composites against oxidation

Yanhui Chu, Qiangang Fu, Hejun Li, Heng Wu, Kezhi Li, Jun Tao, Qin Lei

科研成果: 期刊稿件文章同行评审

53 引用 (Scopus)

摘要

A dense SiC coating toughened by SiC nanowires was prepared on carbon/carbon (C/C) composites using a two-step technique of chemical vapor deposition (CVD) to protect them against oxidation. The morphologies and crystalline structures of the coatings were characterized by scanning electron microscopy, transmission electron microscopy and X-ray diffraction. SiC nanowires played a role in decreasing the size of the cracks and improving the thermal shock resistance of the coating. The result of thermal shock between 1773 K and room temperature for 21 times indicates that, compared with the SiC coating without SiC nanowires, the average size of the cracks in the SiC coating toughened with SiC nanowires reduced from 5 ± 0.5 to 3 ± 0.5 μm. The weight loss of the SiC coated C/C composites decreased from 9.32 to 4.45% by the introduction of SiC nanowires.

源语言英语
页(从-至)189-194
页数6
期刊Ceramics International
38
1
DOI
出版状态已出版 - 1月 2012

指纹

探究 'SiC coating toughened by SiC nanowires to protect C/C composites against oxidation' 的科研主题。它们共同构成独一无二的指纹。

引用此