Pt/HZSM-5 catalyst synthesized by atomic layer deposition for aqueous-phase hydrogenation of levulinic acid to valeric acid
Xiao Min Gu, Bin Zhang, Hao Jie Liang, Hui Bin Ge, Hui Min Yang, Yong Qin