摘要
Preparation of β-SiC nanorods with and without amorphous SiO2 wrapping layers Was achieved by carbothermal reduction of sol-gel derived silica xerogels containing carbon nanoparticles. The β-SiC nanorods with amorphous SiO2 wrapping layers were obtained by carboreduction at 1650°C for 1.5 h, and at the end of 1.5 h the temperature was steeply raised to 1800°C and held for 30 min; they are typically up to 20 μm in length. The diameters of the center thinner β-SiC nanorods within the amorphous SiO2 wrapping layers are in the range 10-30 nm, while the outer diameters of the corresponding amorphous SiO2 wrapping layers are between 20 and 70 nm. The β-SiC nonorods without amorphous SiO2 wrapping layers were produced by carbothermal reduction only at 1650°C for 2.5 h, and their diameters are in agreement with those of the center thinner β-SiC nanorods wrapped in amorphous SiO2 layers. Large quantities of SiC rod nuclei and the nanometer-sized nucleus sites on cabon nanoparticles are both favorable to the formation of much thinner β-SiC nanorods. The formatrion of the outer amorphous SiO2 wrapping layer is from the combination reaction of decomposed SiO vapor and O2.
源语言 | 英语 |
---|---|
页(从-至) | 2533-2538 |
页数 | 6 |
期刊 | Journal of Materials Research |
卷 | 13 |
期 | 9 |
DOI | |
出版状态 | 已出版 - 9月 1998 |