Influences of peparation conditions on melting and reformation behaviors of (Bi,Pb)-2223 core in the Ag-sheathed tape

J. Y. Li, H. L. Zheng, J. G. Li, C. S. Li, Y. F. Lu, L. Zhou

科研成果: 书/报告/会议事项章节会议稿件同行评审

2 引用 (Scopus)

摘要

Three kinds of Ag-sheathed (Bi,Pb)2Sr2Ca 2Cu3O10 ((Bi,Pb)-2223) monofilamentary tapes were fabricated by powder-in-tube (PIT) process under different conditions. The phase evolutions during melting and reformation of (Bi,Pb)-2223 core in them have been investigated by ex-situ X-ray diffraction (XRD) analysis. The short tapes were melted at 855°C, 858°C in 7.5% O2 balanced with argon, and then slowly cooled to 801°C and 804°C at 1.5°C/h, respectively. The results show that the (Bi,Pb)-2223 phase can reform directly from the melt in all three tapes if the appropriate melting temperatures are used. However, the ceramic cores underneath the silver sheath exhibit different melting and recrystalization behaviors, as the differences of phase compositions in the original tapes before melted.

源语言英语
主期刊名Progress in Light Metals, Aerospace Materials and Superconductors
出版商Trans Tech Publications Ltd
1967-1970
页数4
版本PART 4
ISBN(印刷版)0878494324, 9780878494323
DOI
出版状态已出版 - 2007
活动2006 Beijing International Materials Week, 2006 BIMW - International Conference on Superconducting Materials, ICSM 2006 - Beijing, 中国
期限: 25 6月 200630 6月 2006

出版系列

姓名Materials Science Forum
编号PART 4
546-549
ISSN(印刷版)0255-5476
ISSN(电子版)1662-9752

会议

会议2006 Beijing International Materials Week, 2006 BIMW - International Conference on Superconducting Materials, ICSM 2006
国家/地区中国
Beijing
时期25/06/0630/06/06

指纹

探究 'Influences of peparation conditions on melting and reformation behaviors of (Bi,Pb)-2223 core in the Ag-sheathed tape' 的科研主题。它们共同构成独一无二的指纹。

引用此