High temperature wear behavior of Fe-Al coating prepared by high velocity arc spraying

Zi Xin Zhu, Bin Shi Xu, Shi Ning Ma, Wei Min Liu, Wei Zhang

科研成果: 期刊稿件文章同行评审

9 引用 (Scopus)

摘要

Fe-Al intermetallic coating was prepared on a mild steel substrate making use of high velocity arc spraying (HVAS). The high temperature wear behavior of the resulting Fe-Al intermetallic coating against Si3N4 under dry sliding up to 650°C was investigated on a ball-on-disc test rig. The friction and wear mechanisms of the coating were discussed, based on the morphological observation of the worn surface and cross-section on a scanning electron microscope and the elemental composition measurement thereon by means of energy dispersive spectrometry. It was found that the friction coefficient of the coating decreased and the wear resistance significantly increased with increasing testing temperature. This was attributed to the solid lubricity of the oxide protective layer formed on the worn surface by way of tribochemical reactions and to the good ability of the Fe3Al and FeAl intermetallics to retain higher strength and hardness at elevated temperatures. Namely, the Fe3Al and FeAl intermetallics of higher strength and hardness at elevated temperatures made it possible to effectively resist crack initiation, propagation, and fracture, which largely accounted for the excellent wear resistance of the Fe-Al coating sliding against the ceramic counterpart at elevated temperatures. Moreover, the Fe-Al intermetallic coating was dominated by delamination as it slid against the ceramic counterpart at elevated temperatures.

源语言英语
页(从-至)106-110
页数5
期刊Mocaxue Xuebao/Tribology
24
2
出版状态已出版 - 3月 2004
已对外发布

指纹

探究 'High temperature wear behavior of Fe-Al coating prepared by high velocity arc spraying' 的科研主题。它们共同构成独一无二的指纹。

引用此