The microstructure evolution during annealing of Ti–5Al–2Sn–2Zr–4Mo–4Cr alloy was investigated. The results show that for the alloy compressed at 810 °C and 1.0 s−1 deformation amount (height reduction) 20% and 50% and annealed at 810 °C, thermal grooving by penetration of β phase is sufficient during the first 20 min annealing, resulting in a sharp increase in globularization fraction. The globularization fraction continuously increases with the increase of annealing time, and a height reduction of 50% leads to a near globular microstructure after annealing for 4 h. For the alloy with deformation amount of 50% by compressing at 810 °C, 0.01 s−1 and then annealed at 810 °C, thermal grooving is limited during the first 20 min of annealing and large quantities of high-angle grain boundaries (HABs) remain. With long time annealing, the chain-like α grains are developed due to the HABs, termination migration and Ostwald ripening. The present results suggest that a higher strain rate and a larger height reduction are necessary before annealing to achieve a globular microstructure of Ti–5Al–2Sn–2Zr–4Mo–4Cr.

源语言英语
页(从-至)912-919
页数8
期刊Transactions of Nonferrous Metals Society of China (English Edition)
28
5
DOI
出版状态已出版 - 5月 2018

指纹

探究 'Effect of predeformation on globularization of Ti–5Al–2Sn–2Zr–4Mo–4Cr during annealing' 的科研主题。它们共同构成独一无二的指纹。

引用此