Directional growth and thermoelectric properties of the directionally solidified Bi 2Te 3-Sb 2Te 3 ternary alloys

Songke Feng, Shuangming Li, Qinyan Luo, Hengzhi Fu

科研成果: 期刊稿件文章同行评审

1 引用 (Scopus)

摘要

The bulk thermoelectric materials of Bi 2Te 3-Sb 2Te 3 ternary alloy were prepared using a vertical Bridgman method at solidification rates ranging from 5 μm/s to 1000 μm/s. The directionally solidified microstructures with the composition of 25% Bi 2Te 3-75% Sb 2Te 3 alloy were investigated and the corresponding thermoelectric properties were measured. The results shows that the directionally solidified microstructures of 25% Bi 2Te 3-75% Sb 2Te 3 alloy only consist of Bi 0.5Sb 1.5Te 3 single phase. At a low solidification rate of 5 μm/s, the cellular structures appear due to the solid/liquid interface losing its stabilization, and the increase of the solidification rate results in decreasing cellular structures. Additionally, the values of Seebeck coefficient and the resistivity of directionally solidified 25% Bi 2Te 3-75% Sb 2Te 3 alloys tend to a increase with increasing of the solidification rate. Under the solidification rate of 50 μm/s, the Power Factor (PF) of the alloy maintains (4.6-5.01)× 10 -3 W/(K 2 · m) in the temperature range of 300-450 K, and its maximum value reaches 5.01 × 10 -3 W/(K 2 · m) at 350 K. Besides, at a higher solidification rate of 500 μm/s, the maximal PF value can be measured to be 4.5 × 10 -3 W/(K 2 · m). It seems that the Bridgman method employing high temperature gradient with rapid solidification rate is a promising approach for the preparation of thermoelectric materials with high performance. Copyright

源语言英语
页(从-至)894-898
页数5
期刊Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering
41
5
出版状态已出版 - 5月 2012

指纹

探究 'Directional growth and thermoelectric properties of the directionally solidified Bi 2Te 3-Sb 2Te 3 ternary alloys' 的科研主题。它们共同构成独一无二的指纹。

引用此