Creep behaviors of nickel-based single crystal superalloys compact tension specimen at high temperature

Zhixun Wen, Naixian Hou, Zhufeng Yue

科研成果: 书/报告/会议事项章节会议稿件同行评审

6 引用 (Scopus)

摘要

Based on the microstructure change and damage characteristics of single crystal, a two-state-variable crystallographic creep damage constitutive model has been developed to investigate crack growth behaviors of single crystal compact tension specimen at 760°C. for two crack orientations: (001)[100] and (011)[100]. Numerical simulation results show the crack-tip stress fields are dependent on crack crystallographic orientation. Observations performed on the real single crystal specimens reveals that the macroscopic crack growth path appears as zigzag wave. The creep deformation at crack tip takes place in specific slip plane, and the deflection angles of crack initiation direction from the crack plane are 45° or 135° and 53.7° or 127.3° in the crack orientations (001)[100] and (011)[100]. A good agreement between experimental observations and numerical results is found.

源语言英语
主期刊名Advances in Superalloys
1322-1326
页数5
DOI
出版状态已出版 - 2011
活动2010 International Conference on Advances in Materials and Manufacturing Processes, ICAMMP 2010 - Shenzhen, 中国
期限: 6 11月 20108 11月 2010

出版系列

姓名Advanced Materials Research
146-147
ISSN(印刷版)1022-6680

会议

会议2010 International Conference on Advances in Materials and Manufacturing Processes, ICAMMP 2010
国家/地区中国
Shenzhen
时期6/11/108/11/10

指纹

探究 'Creep behaviors of nickel-based single crystal superalloys compact tension specimen at high temperature' 的科研主题。它们共同构成独一无二的指纹。

引用此