Atomistic simulation of nanoindentation on incipient plasticity and dislocation evolution in γ/γ′ phase with interface and void
Biao Yang, Bailin Zheng, Xingjian Hu, Kai Zhang, Yong Li, Pengfei He, Zhufeng Yue