TY - JOUR
T1 - Surface Patterning of Metal Zinc Electrode with an In-Region Zincophilic Interface for High-Rate and Long-Cycle-Life Zinc Metal Anode
AU - Wang, Tian
AU - Xi, Qiao
AU - Yao, Kai
AU - Liu, Yuhang
AU - Fu, Hao
AU - Kavarthapu, Venkata Siva
AU - Lee, Jun Kyu
AU - Tang, Shaocong
AU - Fattakhova-Rohlfing, Dina
AU - Ai, Wei
AU - Yu, Jae Su
N1 - Publisher Copyright:
© The Author(s) 2024.
PY - 2024/2/9
Y1 - 2024/2/9
N2 - The undesirable dendrite growth induced by non-planar zinc (Zn) deposition and low Coulombic efficiency resulting from severe side reactions have been long-standing challenges for metallic Zn anodes and substantially impede the practical application of rechargeable aqueous Zn metal batteries (ZMBs). Herein, we present a strategy for achieving a high-rate and long-cycle-life Zn metal anode by patterning Zn foil surfaces and endowing a Zn-Indium (Zn-In) interface in the microchannels. The accumulation of electrons in the microchannel and the zincophilicity of the Zn-In interface promote preferential heteroepitaxial Zn deposition in the microchannel region and enhance the tolerance of the electrode at high current densities. Meanwhile, electron aggregation accelerates the dissolution of non-(002) plane Zn atoms on the array surface, thereby directing the subsequent homoepitaxial Zn deposition on the array surface. Consequently, the planar dendrite-free Zn deposition and long-term cycling stability are achieved (5,050 h at 10.0 mA cm−2 and 27,000 cycles at 20.0 mA cm−2). Furthermore, a Zn/I2 full cell assembled by pairing with such an anode can maintain good stability for 3,500 cycles at 5.0 C, demonstrating the application potential of the as-prepared ZnIn anode for high-performance aqueous ZMBs. (Figure presented.).
AB - The undesirable dendrite growth induced by non-planar zinc (Zn) deposition and low Coulombic efficiency resulting from severe side reactions have been long-standing challenges for metallic Zn anodes and substantially impede the practical application of rechargeable aqueous Zn metal batteries (ZMBs). Herein, we present a strategy for achieving a high-rate and long-cycle-life Zn metal anode by patterning Zn foil surfaces and endowing a Zn-Indium (Zn-In) interface in the microchannels. The accumulation of electrons in the microchannel and the zincophilicity of the Zn-In interface promote preferential heteroepitaxial Zn deposition in the microchannel region and enhance the tolerance of the electrode at high current densities. Meanwhile, electron aggregation accelerates the dissolution of non-(002) plane Zn atoms on the array surface, thereby directing the subsequent homoepitaxial Zn deposition on the array surface. Consequently, the planar dendrite-free Zn deposition and long-term cycling stability are achieved (5,050 h at 10.0 mA cm−2 and 27,000 cycles at 20.0 mA cm−2). Furthermore, a Zn/I2 full cell assembled by pairing with such an anode can maintain good stability for 3,500 cycles at 5.0 C, demonstrating the application potential of the as-prepared ZnIn anode for high-performance aqueous ZMBs. (Figure presented.).
KW - Aqueous Zn-I batteries
KW - Directional Zn deposition
KW - Surface patterning
KW - Zn metal anode
UR - http://www.scopus.com/inward/record.url?scp=85184852537&partnerID=8YFLogxK
U2 - 10.1007/s40820-024-01327-2
DO - 10.1007/s40820-024-01327-2
M3 - 文章
AN - SCOPUS:85184852537
SN - 2311-6706
VL - 16
JO - Nano-Micro Letters
JF - Nano-Micro Letters
IS - 1
M1 - 112
ER -