Strengthening mechanism of a Ni-based superalloy prepared by laser powder bed fusion: The role of cellular structure

Xinxin Liu, Rui Hu, Chenyu Yang, Xian luo, Yanhao Hou, Jie Bai, Rui Ma

Research output: Contribution to journalArticlepeer-review

22 Scopus citations

Fingerprint

Dive into the research topics of 'Strengthening mechanism of a Ni-based superalloy prepared by laser powder bed fusion: The role of cellular structure'. Together they form a unique fingerprint.