Abstract
The (Fe88Si12)95Al5 alloy was prepared by an aluminothermics. The (Fe88Si12)95Al5 alloy is composed of spheroidic a-Fe(Si,Al) precipitate with size of 20-50 nm and y-Fe(Si,Al) matrix. The yield strength and fracture strain in compression of the (Fe 88Si12)95Al5 alloy are 1500 MPa and 23% respectively. The shear bands propagating in the compressive deformation are arrested by the precipitation particles that resulted in large ductility and high strength simultaneously.
Original language | English |
---|---|
Pages (from-to) | 1482-1484 |
Number of pages | 3 |
Journal | Materials Science and Technology |
Volume | 27 |
Issue number | 9 |
DOIs | |
State | Published - Sep 2011 |
Externally published | Yes |
Keywords
- (FeSi)Al alloy
- Aluminothermics
- Microstructure
- Precipitation hardening