Grain growth and fatigue behaviors of GH4169 superalloy subjected to excessive ultrasonic surface rolling process

Jing Yang, Daoxin Liu, Zhencheng Ren, Yinglin Zhi, Xiaohua Zhang, Ruiming Zhao, Dan Liu, Xingchen Xu, Kaifa Fan, Chengsong Liu, Hao Zhang, Chang Ye

Research output: Contribution to journalArticlepeer-review

52 Scopus citations

Fingerprint

Dive into the research topics of 'Grain growth and fatigue behaviors of GH4169 superalloy subjected to excessive ultrasonic surface rolling process'. Together they form a unique fingerprint.

Engineering

Material Science