FEM analysis on the heat spinning for Ni-Cr-W-Mo superalloy workpiece with strange shape

Zhen An, Jinshan Li, Rui Hu, Jian Wang, Xinchao Jia, Lian Zhou

Research output: Contribution to journalArticlepeer-review

4 Scopus citations

Fingerprint

Dive into the research topics of 'FEM analysis on the heat spinning for Ni-Cr-W-Mo superalloy workpiece with strange shape'. Together they form a unique fingerprint.