N2 - The thermos-structural materials with high strength and high temperature water-oxygen corrosion resistance are urgently needed in aero-space fields. SiC whisker reinforced SiC matrix (SiCw/SiC) composites are the ideal candidate materials for their excellent mechanical properties and thermostability. However, the poor resistance to water-oxygen corrosion ability of SiC matrix limits their further application. In this work, a novel SiCw/SiC–Si–Y composites were first prepared by infiltrating silicon-yttrium (Si–Y) alloy into SiCw/C preform via reactive melt infiltration method. The as-obtained composites not only show the excellent mechanical properties (σF = 363 MPa, KⅠC = 9.14 MPa m1/2), and more importantly after water-oxygen corrosion of 20 h at such temperature as high as 1500 °C, the strength and toughness retention of the composites can reach 106.1% and 103.6%, respectively. The SiCw/SiC–Si–Y composites developed in this paper have a great potential as a new high-performance thermos-structural material for aero-space applications.
AB - The thermos-structural materials with high strength and high temperature water-oxygen corrosion resistance are urgently needed in aero-space fields. SiC whisker reinforced SiC matrix (SiCw/SiC) composites are the ideal candidate materials for their excellent mechanical properties and thermostability. However, the poor resistance to water-oxygen corrosion ability of SiC matrix limits their further application. In this work, a novel SiCw/SiC–Si–Y composites were first prepared by infiltrating silicon-yttrium (Si–Y) alloy into SiCw/C preform via reactive melt infiltration method. The as-obtained composites not only show the excellent mechanical properties (σF = 363 MPa, KⅠC = 9.14 MPa m1/2), and more importantly after water-oxygen corrosion of 20 h at such temperature as high as 1500 °C, the strength and toughness retention of the composites can reach 106.1% and 103.6%, respectively. The SiCw/SiC–Si–Y composites developed in this paper have a great potential as a new high-performance thermos-structural material for aero-space applications.
KW - High temperature
KW - SiC whisker
KW - Water-oxygen corrosion
KW - Yttrium-modified SiC matrix
UR - http://www.scopus.com/inward/record.url?scp=85154037375&partnerID=8YFLogxK
U2 - 10.1016/j.jmrt.2023.04.150
DO - 10.1016/j.jmrt.2023.04.150
M3 - 文章
AN - SCOPUS:85154037375
SN - 2238-7854
VL - 24
SP - 5876
EP - 5882
JO - Journal of Materials Research and Technology
JF - Journal of Materials Research and Technology
ER -