Abstract
Nano-yttria powder can be synthesized by yttrium citrate-urea precursor, combusted at 600°C in air. The CVD SiC coated on graphite (CVD SiC/Graphite) infiltrated by the yttrium citrate-urea precursor, combusted at of 600°C, and then sintered at 1450°C, the thin yttria film can be achieved. The SEM morphology and EDS result of the thin yttria film show a mass of needle-shaped pining into the CVD SiC layer, which improves the combination of CVD SiC layer and wash yttria coating. Therefore, it is an effective transition layer between CVD SiC coating and wash yttria layer.
Original language | English |
---|---|
Pages (from-to) | 653-656 |
Number of pages | 4 |
Journal | Key Engineering Materials |
Volume | 334-335 II |
DOIs | |
State | Published - 2007 |
Keywords
- Multi-layer coating
- Nanopowder
- SiC/graphite
- Yttria