Cracking mechanism of Hastelloy X superalloy during directed energy deposition additive manufacturing

Bojing Guo, Yashan Zhang, Zhongsheng Yang, Dingcong Cui, Feng He, Junjie Li, Zhijun Wang, Xin Lin, Jincheng Wang

Research output: Contribution to journalArticlepeer-review

106 Scopus citations

Fingerprint

Dive into the research topics of 'Cracking mechanism of Hastelloy X superalloy during directed energy deposition additive manufacturing'. Together they form a unique fingerprint.

Material Science