摘要
Nb–Si based alloys are directionally solidified at the withdrawal rates of 100, 500 and 1000 μm/s respectively. At the withdrawal rate of 100 μm/s, the eutectic presents well-coupled lamellar structure. Besides, NbSS and γ-(Nb, X)5Si3 phases are well oriented along [111]Nb and [0001]γ crystallographic orientations respectively and the crystallographic orientation relationship of <111>Nb//<0001>γ, {110}Nb//{101‾0}γ is obeyed. When the withdrawal rate reaches to 500 μm/s, the eutectic begins to transform into irregular fibrous structure and no crystallographic orientation relationship can be detected, and it is caused by the variation in growth direction of NbSS phases from [111]Nb to [100]Nb.
源语言 | 英语 |
---|---|
文章编号 | 153023 |
期刊 | Journal of Alloys and Compounds |
卷 | 819 |
DOI | |
出版状态 | 已出版 - 5 4月 2020 |