摘要
Cycle characteristics of conductive sulfur-containing materials (CSMs) synthesized by heating the mixture of polyacrylonitrile and elemental sulfur at a wider temperature region from 250 to 800 °C are presented. The cyclability is improved remarkably for CSMs obtained above 400 °C. A stable capacity of CSM prepared at 450 °C maintains about 470 mAh g-1 and the capacity retention remains ca. 90% after near 380 cycles. Fourier-transform infrared spectroscopy (FTIR) and Raman characterizations disclose that the fundamental chemical structure of CSMs is composed of dehydropyridine type matrix with SS bond in side-chain. Such unique structure and better electrical conductivity ensure the excellent cycle performance of the prepared CSMs.
源语言 | 英语 |
---|---|
页(从-至) | 335-339 |
页数 | 5 |
期刊 | Journal of Power Sources |
卷 | 146 |
期 | 1-2 |
DOI | |
出版状态 | 已出版 - 26 8月 2005 |
已对外发布 | 是 |