Solidification microstructure of Rene95 superalloy by laser metal forming

Li Ping Feng, Xin Lin, Da Rong Chen, Wei Dong Huang, Hai Ou Yang

科研成果: 期刊稿件文章同行评审

源语言英语
页(从-至)79
页数1
期刊Journal Wuhan University of Technology, Materials Science Edition
19
SUPPL.
出版状态已出版 - 11月 2004

引用此