TY - JOUR
T1 - Preparation, ablation behavior and mechanism of C/C-ZrC-SiC and C/C-SiC composites
AU - Zhao, Zhigang
AU - Li, Kezhi
AU - Li, Wei
AU - Liu, Qing
AU - Kou, Gang
AU - Zhang, Yulei
N1 - Publisher Copyright:
© 2018 Elsevier Ltd and Techna Group S.r.l.
PY - 2018/5
Y1 - 2018/5
N2 - ZrC precursor was synthesized by a solution approach using ZrOCl2·8H2O, acetylacetonate, glycerol and boron-modified phenolic resin. A ZrC yield of ~ 40.56 wt% was obtained at 1500 °C in the C/Zr molar ratio of 1:1. C/C-ZrC-SiC composites were fabricated by a combined processes of chemical vapor infiltration (CVI) and precursor infiltration and pyrolysis (PIP) using the synthesized ZrC precursor. For comparison, C/C-SiC composites were prepared by CVI. Thermogravimetric analysis showed that C/C-ZrC-SiC composites exhibited better oxidation resistance than C/C-SiC composites. After oxyacetylene torch ablation, the mass ablation rate of C/C-ZrC-SiC composites was 9.23% lower than that of C/C-SiC composites. The porous ZrO2 skeleton in the ablation center was prone to be peeled off by the flame flow, resulting in the higher linear ablation rate of C/C-ZrC-SiC composites. The oxide layers of ZrO2 and SiO2 were formed on the transition and brim region of C/C-ZrC-SiC composites and acted as effective heat and oxygen barriers. For C/C-SiC composites, the C-SiC matrix was severely depleted in the ablation center and the formed SiO2 layer in the brim region could protect the matrix against further ablation.
AB - ZrC precursor was synthesized by a solution approach using ZrOCl2·8H2O, acetylacetonate, glycerol and boron-modified phenolic resin. A ZrC yield of ~ 40.56 wt% was obtained at 1500 °C in the C/Zr molar ratio of 1:1. C/C-ZrC-SiC composites were fabricated by a combined processes of chemical vapor infiltration (CVI) and precursor infiltration and pyrolysis (PIP) using the synthesized ZrC precursor. For comparison, C/C-SiC composites were prepared by CVI. Thermogravimetric analysis showed that C/C-ZrC-SiC composites exhibited better oxidation resistance than C/C-SiC composites. After oxyacetylene torch ablation, the mass ablation rate of C/C-ZrC-SiC composites was 9.23% lower than that of C/C-SiC composites. The porous ZrO2 skeleton in the ablation center was prone to be peeled off by the flame flow, resulting in the higher linear ablation rate of C/C-ZrC-SiC composites. The oxide layers of ZrO2 and SiO2 were formed on the transition and brim region of C/C-ZrC-SiC composites and acted as effective heat and oxygen barriers. For C/C-SiC composites, the C-SiC matrix was severely depleted in the ablation center and the formed SiO2 layer in the brim region could protect the matrix against further ablation.
KW - Ablation
KW - Carbon/carbon composites
KW - Microstructure
KW - Precursor infiltration and pyrolysis
UR - http://www.scopus.com/inward/record.url?scp=85041625940&partnerID=8YFLogxK
U2 - 10.1016/j.ceramint.2018.01.125
DO - 10.1016/j.ceramint.2018.01.125
M3 - 文章
AN - SCOPUS:85041625940
SN - 0272-8842
VL - 44
SP - 7481
EP - 7490
JO - Ceramics International
JF - Ceramics International
IS - 7
ER -