Ordering Transformation and Age Hardening in a Ni-Cr-W Superalloy

Xiangyu Gao, Rui Hu, Xiaolin Li, Gongliao Luo, Jinshan Li, Hengzhi Fu

科研成果: 期刊稿件文章同行评审

5 引用 (Scopus)

摘要

The microstructural changes occurring in a Ni-Cr-W superalloy during prolonged exposure to proper temperature have been investigated using transmission electron microscopy. It is demonstrated that nanometer-sized C11b (Pt2Mo-type) and DO22 superlattices can precipitate in the Ni-Cr-W alloy by means of a simple aging treatment at temperatures varying in the range of 773 K to 973 K (500 °C to 700 °C). The mechanism of transformation to long-range order has been revealed to accord with continuous mode based on transmission electron microscopy results and variation trend in Vickers microhardness. No signs of overaging and coarsening of C11b and DO22 phases with further aging have been found, which indicates that both of them have a high-thermal stability. The orientation relationships and interfaces between C11b/DO22 precipitates and Ni-based matrix have been investigated by high-resolution transmission electron microscopy, and the results reveal that the interfaces between C11b/DO22 precipitates and surrounding matrix are coherent at the atomic scale. Because of the high-density nanometer-sized C11b/DO22 precipitates, the microhardness of the alloy is improved remarkably.

源语言英语
页(从-至)5907-5917
页数11
期刊Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science
47
12
DOI
出版状态已出版 - 1 12月 2016

指纹

探究 'Ordering Transformation and Age Hardening in a Ni-Cr-W Superalloy' 的科研主题。它们共同构成独一无二的指纹。

引用此