title = "Microstructure evolution of the Ti-6.62Al-5.14Sn-1.82Zr alloy in the superplastic compression",
abstract = "Superplastic compression of the Ti-6.62Al-5.14Sn-1.82Zr alloy were carried out at a Thermecmaster-Z simulator at deformation temperatures of 960°C, 980°C, 1000°C and 1020°C, strain rate of 0.001 s-1, 0.01 s-1 and 0.1 s-1, and height reduction of 50%, 60% and 70%. The a phase decreases with the increasing of deformation temperature, and the grain size of α phase has a slight variation with the deformation temperature. The strain rate affects both the morphologies and the grain size of α phase, and the optimal strain rate makes the grains be fine. The optimal height reduction also makes the α phase be fine and well distributed on the matrix of Ti-6.62Al-5.14Sn-1.82Zr alloy after superplastic compression.",
keywords = "Microstructure, Superplastic compression, Titanium alloy",
author = "Li, {M. Q.} and Pan, {H. S.} and Lin, {Y. Y.}",
year = "2007",
doi = "10.4028/0-87849-435-9.379",
language = "英语",
isbn = "0878494359",
series = "Materials Science Forum",
publisher = "Trans Tech Publications Ltd",
pages = "379--382",
booktitle = "Superplasticity in Advanced Materials - ICSAM 2006 - Proceedings of the 9th International Conference on Superplasticity in Advanced Materials",
note = "9th International Conference on Superplasticity in Advanced Materials, ICSAM 2006 ; Conference date: 23-06-2006 Through 26-06-2006",
}