TY - JOUR
T1 - Microstructural transition of Nb-Si based alloy during directional solidification upon abruptly decreasing withdrawal rate
AU - Fang, Xin
AU - Guo, Xiping
AU - Qiao, Yanqiang
N1 - Publisher Copyright:
© 2020 Elsevier B.V.
PY - 2020/11/30
Y1 - 2020/11/30
N2 - Multi-element Nb-Si based alloys are directionally solidified upon abruptly decreasing withdrawal rate from 100 to 10 μm/s and at the constant withdrawal rate of 10 μm/s respectively. With increasing solidification distance after decreasing withdrawal rate, the volume fraction of primary γ-(Nb, X)5Si3 increase from 6.7% to 13.9% firstly and finally decreases to 10.5%, which is similar with the variation in Si concentration of the alloy. On the other hand, the volume fraction of γ-(Nb, X)5Si3 in eutectic cells decreases from 36.7% to 28.5% gradually after abruptly deceasing withdrawal rate. After abruptly decreasing withdrawal rate, the average size of primary γ-(Nb, X)5Si3 increases from 31.1 to 58.0 μm, and the average size of eutectic cells increases from 42.5 μm to 128.2 μm, and the average interphase spacing increases from 1.9 μm to 4.4 μm. The phase proportion, microstructural sizes, hardness and elastic modulus of constituent phases in Nb-Si based alloys directionally solidified upon abruptly decreasing withdrawal rate are similar with that of the alloy at a constant withdrawal rate of 10 μm/s. The average hardness and elastic modulus for NbSS are about 6 and 150 GPa respectively, for γ-(Nb, X)5Si3 are 19 and 280 GPa respectively. However, the results of XRD and EBSD show that the coupling degree of eutectics obtained by abruptly decreasing withdrawal rate is better than that at the constant withdrawal rate of 10 μm/s, which indicates that the method of abruptly decreasing withdrawal rate can modify the microstructure.
AB - Multi-element Nb-Si based alloys are directionally solidified upon abruptly decreasing withdrawal rate from 100 to 10 μm/s and at the constant withdrawal rate of 10 μm/s respectively. With increasing solidification distance after decreasing withdrawal rate, the volume fraction of primary γ-(Nb, X)5Si3 increase from 6.7% to 13.9% firstly and finally decreases to 10.5%, which is similar with the variation in Si concentration of the alloy. On the other hand, the volume fraction of γ-(Nb, X)5Si3 in eutectic cells decreases from 36.7% to 28.5% gradually after abruptly deceasing withdrawal rate. After abruptly decreasing withdrawal rate, the average size of primary γ-(Nb, X)5Si3 increases from 31.1 to 58.0 μm, and the average size of eutectic cells increases from 42.5 μm to 128.2 μm, and the average interphase spacing increases from 1.9 μm to 4.4 μm. The phase proportion, microstructural sizes, hardness and elastic modulus of constituent phases in Nb-Si based alloys directionally solidified upon abruptly decreasing withdrawal rate are similar with that of the alloy at a constant withdrawal rate of 10 μm/s. The average hardness and elastic modulus for NbSS are about 6 and 150 GPa respectively, for γ-(Nb, X)5Si3 are 19 and 280 GPa respectively. However, the results of XRD and EBSD show that the coupling degree of eutectics obtained by abruptly decreasing withdrawal rate is better than that at the constant withdrawal rate of 10 μm/s, which indicates that the method of abruptly decreasing withdrawal rate can modify the microstructure.
KW - Abruptly decreasing withdrawal rate
KW - Directional solidification
KW - EBSD
KW - Microstructural transition
KW - Nano-indentation
KW - Nb-Si based Alloys
UR - http://www.scopus.com/inward/record.url?scp=85087132852&partnerID=8YFLogxK
U2 - 10.1016/j.jallcom.2020.156073
DO - 10.1016/j.jallcom.2020.156073
M3 - 文章
AN - SCOPUS:85087132852
SN - 0925-8388
VL - 843
JO - Journal of Alloys and Compounds
JF - Journal of Alloys and Compounds
M1 - 156073
ER -