N2 - MSi2-type multicomponent silicide coatings were prepared on Nb alloys by spark plasma sintering using mixed powders of Mo, Ta, W, Zr, Ti and Si. The coatings were composed of thick outer layers and thin inner layers (interdiffusion zone). A two-phase structure consisting of C11b (Mo,Ta,W,Ti)Si2 and C40 (Ti,Ta,Zr)Si2 was observed in the outer layers of all the coatings sintered for holding times ranging from 15 s to 5 min, but the distribution of these elements in each phase gradually became uniform with increasing holding time. The coatings demonstrated excellent protection during oxidation at 1300 °C for 100 h, and a continuous dense oxide scale mainly composed of ZrSiO4 and SiO2 was generated. The alternation of heating and cooling during oxidation caused cracks to appear at the interface between the outer layer and inner layer due to a mismatch of thermal expansion coefficients. However, crack extension was observed only along the inner layer toward the interior due to the multicomponent structure of the outer layer of the coating. The microstructural development and oxidation behavior of the coatings were discussed.
AB - MSi2-type multicomponent silicide coatings were prepared on Nb alloys by spark plasma sintering using mixed powders of Mo, Ta, W, Zr, Ti and Si. The coatings were composed of thick outer layers and thin inner layers (interdiffusion zone). A two-phase structure consisting of C11b (Mo,Ta,W,Ti)Si2 and C40 (Ti,Ta,Zr)Si2 was observed in the outer layers of all the coatings sintered for holding times ranging from 15 s to 5 min, but the distribution of these elements in each phase gradually became uniform with increasing holding time. The coatings demonstrated excellent protection during oxidation at 1300 °C for 100 h, and a continuous dense oxide scale mainly composed of ZrSiO4 and SiO2 was generated. The alternation of heating and cooling during oxidation caused cracks to appear at the interface between the outer layer and inner layer due to a mismatch of thermal expansion coefficients. However, crack extension was observed only along the inner layer toward the interior due to the multicomponent structure of the outer layer of the coating. The microstructural development and oxidation behavior of the coatings were discussed.
KW - Multicomponent silicide
KW - Nb alloy
KW - Oxidation resistance
KW - Spark plasma sintering
UR - http://www.scopus.com/inward/record.url?scp=85189109650&partnerID=8YFLogxK
U2 - 10.1016/j.ceramint.2024.03.330
DO - 10.1016/j.ceramint.2024.03.330
M3 - 文章
AN - SCOPUS:85189109650
SN - 0272-8842
VL - 50
SP - 22306
EP - 22315
JO - Ceramics International
JF - Ceramics International
IS - 13
ER -