Interfacial microstructure evolution and mechanical properties of FGH98 superalloy TLP joints with BNi-2 interlayer

Wei Guo, Jingru Xin, Ding Hao, Jiangtao Xiong, Jinglong Li

科研成果: 期刊稿件文章同行评审

3 引用 (Scopus)

摘要

FGH98 nickel-based powder metallurgy superalloy was successfully bonded via transient liquid phase (TLP) bonding technique with a BNi-2 interlayer. The typical joint consisted of three characteristic zones including: ASZ composed of multiple silicon borides, ISZ with uniform γ solid solution and dispersed small γ′ phases and DAZ containing multiple kinds of borides which exist within and at grain boundaries. With the increase of bonding temperature and holding time, ASZ was gradually replaced by the ISZ, and eutectic structure disappeared. But excessive temperature or time will cause grain coarsening, deteriorating the joint performance. Under the bonding parameters of 1130 °C −60 min, the joint with optimal shear strength was obtained, which is 882 MPa (94% of the base metal strength). The fracture occurs in the DAZ, which is a mixed fracture.

源语言英语
页(从-至)25-39
页数15
期刊Journal of Materials Research and Technology
30
DOI
出版状态已出版 - 1 5月 2024

指纹

探究 'Interfacial microstructure evolution and mechanical properties of FGH98 superalloy TLP joints with BNi-2 interlayer' 的科研主题。它们共同构成独一无二的指纹。

引用此