摘要
High temperature stability (1100−1500 °C) and oxidation behavior at 1500 °C of the SiOC/HfO2 ceramic nanocomposite were investigated in air. Consumption of free carbon dominated thermal stabilities of the bulk at below 1200 °C. Whereas, the continuous cristobalite scale, rather than HfSiO4, was responsible for the improved oxidation resistance at exceeding 1200 °C. At 1500 °C, HfSiO4, with maximum 30 vol. % concentration for duration of ∼ 15 h, suffered ruptured spherical-bubbles by volatilized species and did not consolidate into a completely protective scale. Thus, the bulk exhibited limited resistance to oxidation at 1500 °C for long-term applications.
源语言 | 英语 |
---|---|
文章编号 | 108866 |
期刊 | Corrosion Science |
卷 | 175 |
DOI | |
出版状态 | 已出版 - 10月 2020 |