摘要
The hydride phase in the Ti-5.6Al-4.8Sn-2.0Zr alloy after hydrogenation was investigated through TEM and XRD analysis. The experimental results show that the phase transition temperature of the hydrogenated Ti-5.6Al-4.8Sn-2.0Zr alloy is decreased approximately by 150-200°C. XRD analysis verifies that the hydrogenation treatment accelerates the phase transition process from α phase to β phase of the Ti-5.6Al-4.8Sn-2.0Zr alloy, so as to decrease the phase transition temperature of the alloy. Meanwhile, TiH2 hydride (δ phase) with strip structure appears in α phase and β phase.
源语言 | 英语 |
---|---|
页(从-至) | 343-345 |
页数 | 3 |
期刊 | Rare Metals |
卷 | 28 |
期 | 4 |
DOI | |
出版状态 | 已出版 - 8月 2009 |