The mechanical and electromagnetic (EM) properties of Si3N 4 ceramic were improved by infiltrating SiC into porous Si 3N4 ceramic by chemical vapor infiltration (CVI). After CVI of SiC, the Si3N4-SiC ceramic possesses improved mechanical properties, high permittivity and dielectric loss, and excellent EM shielding effectiveness and EM absorbing properties compared to Si 3N4 ceramic. The lowest EM reflection loss appears when the thickness of the Si3N4-SiC ceramic equals a quarter-wavelength, and the reflection loss remains unchanged for larger thicknesses.