T1 - CMAS corrosion behavior of interface for EB-PVD Gd2Zr2O7/YSZ thermal barrier coatings
AU - Wang, Yufeng
AU - Fu, Qiangang
AU - Dong, Hao
AU - Zhuo, Xueshi
AU - Liang, Xinghua
AU - Liu, Guo
AU - Huang, Lanxiang
AU - Zhang, Xiaofeng
N1 - Publisher Copyright:
© 2024
PY - 2024/12
Y1 - 2024/12
N2 - Thermal barrier coatings (TBCs) of aero-engine surfaces are facing complex working conditions such as high-temperature oxidation, hot-cold cycling, and CMAS corrosion. Gd2Zr2O7 (GZO)/YSZ bilayer ceramic TBCs are one of the coating systems that have been applied in aero-engine TBCs. One of the failure problems faced by the columnar crystalline bilayer GZO/YSZ TBCs prepared by electron beam-physical vapor deposition (EB-PVD) technology in high-temperature environments is the CMAS high-temperature corrosion problem. In this study, CMAS corrosion tests of GZO/YSZ bilayer structure TBCs were conducted at 1200 °C for 1 h, 2 h and 4 h, respectively. The focus was on exploring the corrosion characteristics and mechanisms of the coating interface and surface after high-temperature corrosion. It was found that CMAS corrosion was dominated at the coating interface, accompanied by coating sintering, resulting in coating spalling at the interface. The coating interface was also analyzed by TEM after 4 h corrosion, and it was found that an apatite phase was formed at the GZO/YSZ interface, which was embedded in the lattice of YSZ. Finally, the corrosion failure mechanism of the GZO/YSZ bilayer structure TBCs was proposed by the above CMAS high-temperature corrosion test.
AB - Thermal barrier coatings (TBCs) of aero-engine surfaces are facing complex working conditions such as high-temperature oxidation, hot-cold cycling, and CMAS corrosion. Gd2Zr2O7 (GZO)/YSZ bilayer ceramic TBCs are one of the coating systems that have been applied in aero-engine TBCs. One of the failure problems faced by the columnar crystalline bilayer GZO/YSZ TBCs prepared by electron beam-physical vapor deposition (EB-PVD) technology in high-temperature environments is the CMAS high-temperature corrosion problem. In this study, CMAS corrosion tests of GZO/YSZ bilayer structure TBCs were conducted at 1200 °C for 1 h, 2 h and 4 h, respectively. The focus was on exploring the corrosion characteristics and mechanisms of the coating interface and surface after high-temperature corrosion. It was found that CMAS corrosion was dominated at the coating interface, accompanied by coating sintering, resulting in coating spalling at the interface. The coating interface was also analyzed by TEM after 4 h corrosion, and it was found that an apatite phase was formed at the GZO/YSZ interface, which was embedded in the lattice of YSZ. Finally, the corrosion failure mechanism of the GZO/YSZ bilayer structure TBCs was proposed by the above CMAS high-temperature corrosion test.
KW - CMAS corrosion
KW - Double ceramic layer
KW - EB-PVD
KW - GdZrO/YSZ
KW - Interface
UR - http://www.scopus.com/inward/record.url?scp=85206938842&partnerID=8YFLogxK
U2 - 10.1016/j.mtcomm.2024.110756
DO - 10.1016/j.mtcomm.2024.110756
M3 - 文章
AN - SCOPUS:85206938842
SN - 2352-4928
VL - 41
JO - Materials Today Communications
JF - Materials Today Communications
M1 - 110756
ER -