N2 - High-temperature titanium alloys are ideal for extreme environments due to their lightweight and high strength at elevated temperatures. Laser direct energy deposition (L-DED) enables the production of high-performance, complex high-temperature titanium alloy components, offering significant potential in the aerospace sector. However, the significant anisotropy in the deposit, caused by the presence of epitaxially grown columnar β grains, severely restricts its further application. Although isotropy has been achieved in L-DED Ti or Ti6Al4V using eutectoid elements, the high-temperature service conditions limit their applicability. This study used a synergistic alloying modification of Si and B to promote the columnar to equiaxed transition (CET) of β grains in L-DED near-α titanium alloy Ti6242S. The effects of Si and B alloying on microstructure evolution and both room- and high-temperature mechanical properties were analyzed. Si and B exhibit a notable mutual replacement effect in promoting CET. The synergistic modification of Si and B effectively prevents the formation of silicide and TiB by reducing their individual contents. Fully equiaxed β grains were achieved in L-DED Ti6242S-0.16Si-0.05B alloy deposit, which exhibited a high yield strength of approximately 900 MPa and 13 % elongation at room temperature. The high-temperature yield strength at 480 °C reached 590 MPa, and the step-creep rupture life increased significantly for the Ti6242S-0.16Si-0.05B alloy deposit at 525 °C under 480 MPa–680 MPa.
AB - High-temperature titanium alloys are ideal for extreme environments due to their lightweight and high strength at elevated temperatures. Laser direct energy deposition (L-DED) enables the production of high-performance, complex high-temperature titanium alloy components, offering significant potential in the aerospace sector. However, the significant anisotropy in the deposit, caused by the presence of epitaxially grown columnar β grains, severely restricts its further application. Although isotropy has been achieved in L-DED Ti or Ti6Al4V using eutectoid elements, the high-temperature service conditions limit their applicability. This study used a synergistic alloying modification of Si and B to promote the columnar to equiaxed transition (CET) of β grains in L-DED near-α titanium alloy Ti6242S. The effects of Si and B alloying on microstructure evolution and both room- and high-temperature mechanical properties were analyzed. Si and B exhibit a notable mutual replacement effect in promoting CET. The synergistic modification of Si and B effectively prevents the formation of silicide and TiB by reducing their individual contents. Fully equiaxed β grains were achieved in L-DED Ti6242S-0.16Si-0.05B alloy deposit, which exhibited a high yield strength of approximately 900 MPa and 13 % elongation at room temperature. The high-temperature yield strength at 480 °C reached 590 MPa, and the step-creep rupture life increased significantly for the Ti6242S-0.16Si-0.05B alloy deposit at 525 °C under 480 MPa–680 MPa.
KW - Columnar to equiaxed transition
KW - L-DED
KW - Mechanical properties
KW - Microstructure evolution
KW - Titanium alloy
UR - http://www.scopus.com/inward/record.url?scp=85218146951&partnerID=8YFLogxK
U2 - 10.1016/j.msea.2025.148076
DO - 10.1016/j.msea.2025.148076
M3 - 文章
AN - SCOPUS:85218146951
SN - 0921-5093
VL - 928
JO - Materials Science and Engineering: A
JF - Materials Science and Engineering: A
M1 - 148076
ER -