TY - JOUR
T1 - A Transition from Fine to Coarse Lamellar Eutectics in the Undercooled Ni-29.8 At. Pct Si Eutectic Alloy
T2 - Experiments and Modeling
AU - Zhang, Fan
AU - Wang, Haifeng
AU - Kolbe, M.
AU - Zhang, Jianbao
AU - Zhou, Qing
AU - Herlach, D. M.
N1 - Publisher Copyright:
© 2019, The Minerals, Metals & Materials Society and ASM International.
PY - 2019/6/15
Y1 - 2019/6/15
N2 - In contrast to the classical eutectic growth models, according to which the eutectic spacing decreases invariably with undercooling, an anomalous transition from fine to coarse lamellar eutectics was found in the undercooled Ni-29.8 at. pct Si eutectic alloy. In this study, the growth kinetics, recalescence processes, and grain orientations were analyzed. A sharp increase of the growth velocity at an undercooling of about 100 K was found. The recalescence front transited in sequence from a diffuse one with tips, to a diffuse one without tips and then to a sharp one. The microstructures changed from a mixture of directional rod-shaped γ-Ni 31 Si 12 grains and fine lamellar eutectics to solely coarse lamellar eutectics. Coarse lamellar eutectics were found to be formed by rapid solidification of primary directional rod-shaped Ni 31 Si 12 intermetallic compound and subsequent epitaxial growth of secondary Ni 2 Si intermetallic compound, being consistent with the predictions of eutectic–dendritic and dendritic growth models. Coarse anomalous eutectics at low undercooling were formed by fragmentation of fine lamellar eutectics and their subsequent coarsening. At high undercooling, they were formed by decoupled-eutectic growth.
AB - In contrast to the classical eutectic growth models, according to which the eutectic spacing decreases invariably with undercooling, an anomalous transition from fine to coarse lamellar eutectics was found in the undercooled Ni-29.8 at. pct Si eutectic alloy. In this study, the growth kinetics, recalescence processes, and grain orientations were analyzed. A sharp increase of the growth velocity at an undercooling of about 100 K was found. The recalescence front transited in sequence from a diffuse one with tips, to a diffuse one without tips and then to a sharp one. The microstructures changed from a mixture of directional rod-shaped γ-Ni 31 Si 12 grains and fine lamellar eutectics to solely coarse lamellar eutectics. Coarse lamellar eutectics were found to be formed by rapid solidification of primary directional rod-shaped Ni 31 Si 12 intermetallic compound and subsequent epitaxial growth of secondary Ni 2 Si intermetallic compound, being consistent with the predictions of eutectic–dendritic and dendritic growth models. Coarse anomalous eutectics at low undercooling were formed by fragmentation of fine lamellar eutectics and their subsequent coarsening. At high undercooling, they were formed by decoupled-eutectic growth.
UR - http://www.scopus.com/inward/record.url?scp=85064533801&partnerID=8YFLogxK
U2 - 10.1007/s11661-019-05221-0
DO - 10.1007/s11661-019-05221-0
M3 - 文章
AN - SCOPUS:85064533801
SN - 1073-5623
VL - 50
SP - 2847
EP - 2859
JO - Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science
JF - Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science
IS - 6
ER -