TY - JOUR
T1 - 核-壳结构Al2O3@CIPs的制备及其抗氧化性能和吸波性能
AU - Yu, Mingfei
AU - Yao, Lunbiao
AU - Qing, Yuchang
AU - Ma, Liya
N1 - Publisher Copyright:
© 2022 Beijing Institute of Aeronautical Materials (BIAM). All rights reserved.
PY - 2022/10
Y1 - 2022/10
N2 - Core-shell Al2O3@carbonyl iron powders (CIPs) were prepared by ball-milling-in-situ oxidation method. The phase composition, mass change and micromorphology of Al2O3@CIPs were analyzed by X-ray diffraction, thermogravimetric analyzer and scanning electron microscopy. The effects of various oxidation temperature on electromagnetic properties and absorbing performance of Al2O3@CIPs were studied. The results show that, as the oxidation temperature increases, the shell of Al2O3@CIPs is damaged to some extent and accompanied by the formation of iron oxides, its permittivity rises first and then declines, while permeability shows a downward trend. Compared with CIPs, Al2O3@CIPs obtained by in-situ oxidation at 400℃ achieve excellent electromagnetic wave absorption performance.The real part of the permittivity is about 15, and the imaginary part is 2.8-4.3. The effective absorption band (< -10 dB) of 3.4 GHz can be obtained under the thickness of 1.8 mm in the X-band, while the Al2O3@CIPs obtained by in-situ oxidation at 450℃ achieve the maximum reflection loss of -30 dB at 11.1 GHz.
AB - Core-shell Al2O3@carbonyl iron powders (CIPs) were prepared by ball-milling-in-situ oxidation method. The phase composition, mass change and micromorphology of Al2O3@CIPs were analyzed by X-ray diffraction, thermogravimetric analyzer and scanning electron microscopy. The effects of various oxidation temperature on electromagnetic properties and absorbing performance of Al2O3@CIPs were studied. The results show that, as the oxidation temperature increases, the shell of Al2O3@CIPs is damaged to some extent and accompanied by the formation of iron oxides, its permittivity rises first and then declines, while permeability shows a downward trend. Compared with CIPs, Al2O3@CIPs obtained by in-situ oxidation at 400℃ achieve excellent electromagnetic wave absorption performance.The real part of the permittivity is about 15, and the imaginary part is 2.8-4.3. The effective absorption band (< -10 dB) of 3.4 GHz can be obtained under the thickness of 1.8 mm in the X-band, while the Al2O3@CIPs obtained by in-situ oxidation at 450℃ achieve the maximum reflection loss of -30 dB at 11.1 GHz.
KW - anti-oxidation property
KW - core-shell AlO@CIPs
KW - microwave ab-sorption
KW - permeability
KW - permittivity
UR - http://www.scopus.com/inward/record.url?scp=85141039117&partnerID=8YFLogxK
U2 - 10.11868/j.issn.1001-4381.2021.000330
DO - 10.11868/j.issn.1001-4381.2021.000330
M3 - 文章
AN - SCOPUS:85141039117
SN - 1001-4381
VL - 50
SP - 111
EP - 117
JO - Cailiao Gongcheng/Journal of Materials Engineering
JF - Cailiao Gongcheng/Journal of Materials Engineering
IS - 10
ER -