The second phases in a burn resistant alloy-Ti40

Zhao Yongqing, Qu Henglei, Zhu Kangying, Wu Huan, Liu Caili, Zhou Lian

Research output: Contribution to journalArticlepeer-review

1 Scopus citations

Abstract

Second phase formation in the burn resistant titanium alloy Ti40(Ti-25V-15Cr-0.2Si) and their effects on properties have been studied. The higher the solution temperature, the higher the concention of second phases . No second phases form if the solution temperature is below 850°C , while rod-like a and some Ti5Si3 phases form above 850°C , The a and Ti5Si3 phases precipitate from Ti40 after solution heat treatment at 910°C followed by aging at 600°C , while only Ti5Si3 phases precipitate during heat treatment at 860°C followed by aging at 600°C. Various shapes of a and Ti5Si3 precipitates form in Ti40 after exposure at 540°C for 100 h, decreasing its thermal stability, then influence on properties at RT is not obvious.

Original languageEnglish
Pages (from-to)417
Number of pages1
JournalXiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering
Volume30
Issue number6
StatePublished - 2001
Externally publishedYes

Keywords

  • Burn resistant titanium alloy
  • Mechanical properties
  • Second phase
  • Ti40