TY - JOUR
T1 - The effect of Z-yarn density on the in-plane shear property of three-dimensional stitched carbon fiber reinforced silicon carbide composites
AU - Xu, Huajie
AU - Zhang, Litong
AU - Cheng, Laifei
N1 - Publisher Copyright:
© 2014 Elsevier Ltd.
PY - 2015/1/6
Y1 - 2015/1/6
N2 - Three types of three-dimensional stitched carbon fiber reinforced silicon carbide composites (3DS C/SiCs) were fabricated by chemical vapor infiltration with the Z-yarn density of 4, 9, and 16stitching/cm2 (S4, S9 and S16). The results showed: 3DS C/SiCs with different Z-yarn densities had identical damage mechanism which was referred to as rigid body sliding. The fracture surfaces of both S4 and S9 lied in the stitched line plane. However, S16 exhibited the fracture morphologies of plane rise. Compared with that of S4, the in-plane shear strengths of S9 and S16 increased by 13.1% and 37.5%, respectively. However, the shear moduli of them decreased by 22.2% and 36.4%. Benefitted from the studies of Turner, a formula was proposed to well predict the in-plane shear strength of 3DS C/SiCs with different Z-yarn density. Although they exhibited low in-plane shear strength, 3K 3DS C/SiCs would not alleviate the notch sensitivity through shear stress redistribution. However, the application of them with lower Z-yarn density should be avoided. The similar conclusions as listed above may be also attained for other Z-reinforced ceramic-matrix composites because 3DS C/SiC is a representative of them.
AB - Three types of three-dimensional stitched carbon fiber reinforced silicon carbide composites (3DS C/SiCs) were fabricated by chemical vapor infiltration with the Z-yarn density of 4, 9, and 16stitching/cm2 (S4, S9 and S16). The results showed: 3DS C/SiCs with different Z-yarn densities had identical damage mechanism which was referred to as rigid body sliding. The fracture surfaces of both S4 and S9 lied in the stitched line plane. However, S16 exhibited the fracture morphologies of plane rise. Compared with that of S4, the in-plane shear strengths of S9 and S16 increased by 13.1% and 37.5%, respectively. However, the shear moduli of them decreased by 22.2% and 36.4%. Benefitted from the studies of Turner, a formula was proposed to well predict the in-plane shear strength of 3DS C/SiCs with different Z-yarn density. Although they exhibited low in-plane shear strength, 3K 3DS C/SiCs would not alleviate the notch sensitivity through shear stress redistribution. However, the application of them with lower Z-yarn density should be avoided. The similar conclusions as listed above may be also attained for other Z-reinforced ceramic-matrix composites because 3DS C/SiC is a representative of them.
KW - A. Ceramic-matrix composites (CMCs)
KW - B. Mechanical properties
KW - C. Damage mechanics
KW - E. Chemical vapor infiltration (CVI)
UR - http://www.scopus.com/inward/record.url?scp=84914100719&partnerID=8YFLogxK
U2 - 10.1016/j.compscitech.2014.11.008
DO - 10.1016/j.compscitech.2014.11.008
M3 - 文章
AN - SCOPUS:84914100719
SN - 0266-3538
VL - 106
SP - 120
EP - 126
JO - Composites Science and Technology
JF - Composites Science and Technology
ER -