TY - JOUR
T1 - Spectroscopic characterization of biosynthesized lead oxide (PbO) nanoparticles and their applications in PVC/graphite-PbO nanocomposites
AU - Raza, Junaid
AU - Hamid, Abdul
AU - Khan, Muhammad
AU - Hussain, Fakhar
AU - Tiehu, Li
AU - Fazil, Perveen
AU - Zada, Amir
AU - Wahab, Zainul
AU - Ali, Amjad
N1 - Publisher Copyright:
© 2022 Walter de Gruyter GmbH, Berlin/Boston.
PY - 2022/5/1
Y1 - 2022/5/1
N2 - Extract of Hibiscus rosa-sinensis plants was used for the green synthesis of PbO nanoparticles. The prepared nanoparticles were conformed with the help of SEM, X-ray diffraction, FTIR and UV-visible spectroscopy. The prepared PbO nanoparticles were dispersed in deionized water and mixed with graphite to get graphite-PbO (G-PbO) filler. Seven different nanocomposite membranes with variable compositions (5, 10, 15, 20, 25, 30 and 35%) of PVC/G-PbO were prepared in tetrahydrofuran (THF) solvent using solution casting method. Different physiochemical parameters of the nanocomposite membranes studied included morphology, porosity, density, water uptake, swelling degree, electrical conductivity and proton adsorption capacity. All these physiochemical parameters were compared with pure PVC membranes available in literature. It was found that the addition of G-PbO filler in PVC polymer improved all the physiochemical properties except density. PVC/G-PbO membranes showed 42.65 times more electrical conductivity and 5.90 times more ion adsorption capacities compare to pure PVC membranes.
AB - Extract of Hibiscus rosa-sinensis plants was used for the green synthesis of PbO nanoparticles. The prepared nanoparticles were conformed with the help of SEM, X-ray diffraction, FTIR and UV-visible spectroscopy. The prepared PbO nanoparticles were dispersed in deionized water and mixed with graphite to get graphite-PbO (G-PbO) filler. Seven different nanocomposite membranes with variable compositions (5, 10, 15, 20, 25, 30 and 35%) of PVC/G-PbO were prepared in tetrahydrofuran (THF) solvent using solution casting method. Different physiochemical parameters of the nanocomposite membranes studied included morphology, porosity, density, water uptake, swelling degree, electrical conductivity and proton adsorption capacity. All these physiochemical parameters were compared with pure PVC membranes available in literature. It was found that the addition of G-PbO filler in PVC polymer improved all the physiochemical properties except density. PVC/G-PbO membranes showed 42.65 times more electrical conductivity and 5.90 times more ion adsorption capacities compare to pure PVC membranes.
KW - adsorption capacity
KW - electrical conductivity
KW - nanocomposite membranes
KW - PbO nanoparticles
KW - physiochemical properties
UR - http://www.scopus.com/inward/record.url?scp=85126563174&partnerID=8YFLogxK
U2 - 10.1515/zpch-2021-3152
DO - 10.1515/zpch-2021-3152
M3 - 文章
AN - SCOPUS:85126563174
SN - 0942-9352
VL - 236
SP - 619
EP - 636
JO - Zeitschrift fur Physikalische Chemie
JF - Zeitschrift fur Physikalische Chemie
IS - 5
ER -