TY - JOUR
T1 - Magnetic and electromagnetic properties of Pr doped strontium ferrite/polyaniline composite film
AU - Huang, Ying
AU - Li, Yuqing
AU - Wang, Yan
PY - 2014/11
Y1 - 2014/11
N2 - This paper reported three acid (including hydrochloric acid HCl, p-toluenesulfonic acid PTS and D-camphor-10-acid CSA) doped SrPr 0.2Fe11.8O19/PANI composite film and the HCl-PANI film prepared by a sol-gel method and in-situ oxidative polymerization. The characteristics of the film phase structure, surface morphology, conductivity and magnetic and electromagnetic properties were studied by using XRD, XPS, FESEM, four-probe tester, VSM and Vector Network Analyzer. The resistivity of organic acid doped composite films is higher than that of the HCl doped one. The saturation and remanent magnetization of PTS and HCl doped composite films are greater than the CSA-doped one; however, the coercivity of the three acid doped composite films is basically 5546 Oe. The saturation magnetization, remanent magnetization and coercivity of SrPr 0.2Fe11.8O19 film are greater than those of the SrPr0.2Fe11.8O19-PANI composite film. In the frequency range of 8-12 GHz, the dielectric loss of HCl-PANI film is the maximum, and the dielectric loss of SrPr0.2Fe11.8O 19 film is the minimum; the magnetic loss of the four films is in descending order as SrPr0.2Fe11.8O19 film, PrSrM/(HCl-PANI) composite film, PrSrM/(CSA-PANI) and HCl-PANI film.
AB - This paper reported three acid (including hydrochloric acid HCl, p-toluenesulfonic acid PTS and D-camphor-10-acid CSA) doped SrPr 0.2Fe11.8O19/PANI composite film and the HCl-PANI film prepared by a sol-gel method and in-situ oxidative polymerization. The characteristics of the film phase structure, surface morphology, conductivity and magnetic and electromagnetic properties were studied by using XRD, XPS, FESEM, four-probe tester, VSM and Vector Network Analyzer. The resistivity of organic acid doped composite films is higher than that of the HCl doped one. The saturation and remanent magnetization of PTS and HCl doped composite films are greater than the CSA-doped one; however, the coercivity of the three acid doped composite films is basically 5546 Oe. The saturation magnetization, remanent magnetization and coercivity of SrPr 0.2Fe11.8O19 film are greater than those of the SrPr0.2Fe11.8O19-PANI composite film. In the frequency range of 8-12 GHz, the dielectric loss of HCl-PANI film is the maximum, and the dielectric loss of SrPr0.2Fe11.8O 19 film is the minimum; the magnetic loss of the four films is in descending order as SrPr0.2Fe11.8O19 film, PrSrM/(HCl-PANI) composite film, PrSrM/(CSA-PANI) and HCl-PANI film.
KW - Acid doped
KW - Composite film
KW - Electromagnetic property
KW - Magnetic property
KW - Polyaniline
KW - Strontium ferrite
UR - http://www.scopus.com/inward/record.url?scp=84902204663&partnerID=8YFLogxK
U2 - 10.1016/j.jmmm.2014.05.030
DO - 10.1016/j.jmmm.2014.05.030
M3 - 文章
AN - SCOPUS:84902204663
SN - 0304-8853
VL - 368
SP - 133
EP - 138
JO - Journal of Magnetism and Magnetic Materials
JF - Journal of Magnetism and Magnetic Materials
ER -