Joining of surface modified carbon/carbon composites and LAS glass ceramic

Xiaoqiu Lin, Kezhi Li, Hejun Li, Fengtao Lan

Research output: Contribution to journalArticlepeer-review

7 Scopus citations

Abstract

Carbon/carbon (C/C) composites modified with SiC-MoSi2 coating are joined to Li2CO3 -Al2O3-SiO2 (LAS) glass ceramic using MgO-Al2O3-SiO2 (MAS) glass. The effects of joining temperature, joining pressure, and holding time on the shear strength of the sample are studied. The optimal technological parameters obtained by orthogonal experiments are 1200°C, 20 MPa, and 15 min. Under these conditions, the shear strength of the joined sample is up to 30 MPa. The microstructure of the interfaces is analyzed by scanning electron microscope (SEM), energy disperse spectroscopy (EDS), and backscattered electron image (BEI). Results show that Si and C elements distribute in a gradient in the interface, while an interlayer about of 15 μm is produced which accelerates the joining of SiC-MoSi2 coating and C/C composite. Moreover, C/C(SiC-MoSi2)/MAS/LAS interfaces are formed due to the interdiffusion that occurrs at the interfaces between the glass and SiC-MoSi2 coating and LAS glass ceramic, which contributes to the superior joining of interfaces.

Original languageEnglish
Pages (from-to)380-384
Number of pages5
JournalHangkong Xuebao/Acta Aeronautica et Astronautica Sinica
Volume30
Issue number2
StatePublished - Feb 2009

Keywords

  • Carbon/carbon composites
  • Joining
  • LAS glass ceramic
  • MAS glass
  • Shear strength