N2 - Before the preparation of MoSi2–CrSi2–SiC–Si coating, blasting treatment of carbon/carbon (C/C) composites, as a surface modification method, was conducted under oxyacetylene torch. MoSi2–CrSi2–SiC–Si coating was prepared on the treated C/C composites by pack cementation, where an interlock interface was formed between the coating and the C/C substrate. After blasting treatment, the thermal expansion coefficient mismatch between the coating and C/C substrate was alleviated efficiently, and the bonding strength of the coating was increased by 45.6% and reached 26.2 MPa. To simulate the real working condition, thermal cycling test was conducted under oxyacetylene torch from 1600 °C to room temperature to construct an environment of combustion gas erosion. Due to the improvement of bonding strength and the alleviation of thermal expansion coefficient mismatch between the coating and the C/C substrate, thermal cycling performance of MoSi2–CrSi2–SiC–Si coating was enhanced. After 25 thermal cycles, the mass loss of the coated C/C composites without blasting treatment was up to 2.4%, and the C/C substrate was partially exposed. In contrast, the mass loss of the coated C/C composites with blasting treatment was only 1.1%.
AB - Before the preparation of MoSi2–CrSi2–SiC–Si coating, blasting treatment of carbon/carbon (C/C) composites, as a surface modification method, was conducted under oxyacetylene torch. MoSi2–CrSi2–SiC–Si coating was prepared on the treated C/C composites by pack cementation, where an interlock interface was formed between the coating and the C/C substrate. After blasting treatment, the thermal expansion coefficient mismatch between the coating and C/C substrate was alleviated efficiently, and the bonding strength of the coating was increased by 45.6% and reached 26.2 MPa. To simulate the real working condition, thermal cycling test was conducted under oxyacetylene torch from 1600 °C to room temperature to construct an environment of combustion gas erosion. Due to the improvement of bonding strength and the alleviation of thermal expansion coefficient mismatch between the coating and the C/C substrate, thermal cycling performance of MoSi2–CrSi2–SiC–Si coating was enhanced. After 25 thermal cycles, the mass loss of the coated C/C composites without blasting treatment was up to 2.4%, and the C/C substrate was partially exposed. In contrast, the mass loss of the coated C/C composites with blasting treatment was only 1.1%.
KW - Blasting treatment
KW - C/C composites
KW - Coating
KW - Thermal cycles
UR - http://www.scopus.com/inward/record.url?scp=84973559157&partnerID=8YFLogxK
U2 - 10.1016/j.ceramint.2016.06.008
DO - 10.1016/j.ceramint.2016.06.008
M3 - 文章
AN - SCOPUS:84973559157
SN - 0272-8842
VL - 42
SP - 14021
EP - 14027
JO - Ceramics International
JF - Ceramics International
IS - 12
ER -