T1 - Deformation Behavior and Microstructural Evolution Coordinated Regulation by Compression Deformation for Metastable Ti Alloy
AU - Wang, Xueli
AU - Jia, Penglai
AU - Wang, Taoqin
AU - Li, Fuguo
AU - Wang, Qiang
N1 - Publisher Copyright:
© 2024 by the authors.
PY - 2024/12
Y1 - 2024/12
N2 - In this paper, in order to investigate the harmonious relationship between the compression deformation behavior of metastable β titanium alloy and the microstructure evolution, the β solution-treated Ti-10V-2Fe-3Al (Ti-1023) alloy was compressed at room temperature and its deformation behavior was analyzed. Optical microscopy (OM) and field emission electron microscopy (FESEM) were used to study the microstructure evolution of alloys at different strain rates. The results show that the stress-induced martensite transformation (SIMT) is more easily activated by low strain rate compression deformation, which is conducive to improving its comprehensive mechanical properties. With the decrease in strain rate, the α″ martensite content increases significantly, the average grain size decreases substantially, and the Low Angle Grain Boundary (LAGB) volume fraction decreases correspondingly. In addition, after compression at different strain rates, the misorientation angle (MA) of the β matrix is mainly concentrated in the LAGBs. The change is small with the decrease in strain rate, but the α″ martensite orientation difference angle shows some peaks, which are ~60°, ~85°, and ~95°, respectively. Simultaneously, the strain rate has an important effect on the content and type of martensitic twins. Finally, the fracture morphology analysis shows that with the increase in strain rate, the fracture mode changes from ductile fracture to brittle fracture. The fracture surface presents a significantly elongated cavity along the direction of maximum shear stress.
AB - In this paper, in order to investigate the harmonious relationship between the compression deformation behavior of metastable β titanium alloy and the microstructure evolution, the β solution-treated Ti-10V-2Fe-3Al (Ti-1023) alloy was compressed at room temperature and its deformation behavior was analyzed. Optical microscopy (OM) and field emission electron microscopy (FESEM) were used to study the microstructure evolution of alloys at different strain rates. The results show that the stress-induced martensite transformation (SIMT) is more easily activated by low strain rate compression deformation, which is conducive to improving its comprehensive mechanical properties. With the decrease in strain rate, the α″ martensite content increases significantly, the average grain size decreases substantially, and the Low Angle Grain Boundary (LAGB) volume fraction decreases correspondingly. In addition, after compression at different strain rates, the misorientation angle (MA) of the β matrix is mainly concentrated in the LAGBs. The change is small with the decrease in strain rate, but the α″ martensite orientation difference angle shows some peaks, which are ~60°, ~85°, and ~95°, respectively. Simultaneously, the strain rate has an important effect on the content and type of martensitic twins. Finally, the fracture morphology analysis shows that with the increase in strain rate, the fracture mode changes from ductile fracture to brittle fracture. The fracture surface presents a significantly elongated cavity along the direction of maximum shear stress.
KW - martensitic twinning
KW - metastable β titanium alloy
KW - microscopic morphology
KW - strain rate
KW - stress-induced martensite transformation
UR - http://www.scopus.com/inward/record.url?scp=85213260219&partnerID=8YFLogxK
U2 - 10.3390/ma17246145
DO - 10.3390/ma17246145
M3 - 文章
AN - SCOPUS:85213260219
SN - 1996-1944
VL - 17
JO - Materials
JF - Materials
IS - 24
M1 - 6145